Table of content
- Rockstar 400 Plate Specification
- Rockstar 400 Wear Plate Sizes in Stock
- Available Thickness Of Rockstar 400 BHN Plate
- Ready to Dispatch Stock Of Rockstar 400 Steel Plate
- Rockstar 400 Chemical Composition
- Rockstar 400 Mechanical Properties
- Application Of Rockstar 400 Abrasion Resistant Steel Plate
- Rockstar 400 Liner Plate Standards and Dimensions
- 400 BHN Rockstar Plates Hardness Level
- Welding Method Of Rockstar 400 Liner Plate
- Rockstar 400lt Plate Delivery Condition
- Key Characteristics Of Rockstar High Strength Steel Plate
- Rockstar 400 Hot Rolled Plate Tensile Properties
- Heat Treatment Of Rockstar 400 Wear Resistant Steel Plate
- Rockstar 400 Wear Plate Dimensional Tolerances
- Welding Method Of Rockstar 400 Plate
- Rockstar 400 Low-Temperature Steel Plate Thermal Cutting
Rockstar 400 BHN Plate Manufacturer in India With Hardness 360 to 430 BHN

| Thickness | Width | Length |
|---|---|---|
| 8 to 60mm | 2000 to 2500 mm | As Per Client Requirement |
| Heat Treatment | Brand | Hardness |
| Quenched and Tempered | Arcelor Mittal Nippon Steel India Private Ltd. | 360 to 430 BHN |
| NDT | Welding method | Manufacturing method |
| Ultrasonic test as per SA578 LEVEL-B |
|
|
| BIS Certification | Certification | Standards |
| IS18809_ISAR_400 | EN 10204-3.2 Duly inspected by M/s. Bureau Veritas. | EN 10029: 1991 EN 10163-2: 2004 |
| Value added services | Cutting method | Packaging |
|
|
As Per Client Requirement |
| Documentation | Delivery schedule | Features |
|
Immediate |
|
Supplier Of AMNS Make Rockstar 400 Abrasion Resistant Steel Plate in Mumbai With Width 2,000 to 2,500mm At Factory Price

Rockstar 400 BHN Plate

Rockstar 400 Abrasion Resistant Steel Plate

Rockstar 400 Wear Plate
| Sizes in mm | ||||
|---|---|---|---|---|
| 8 mm | 10 mm | 12 mm | 14 mm | 16 mm |
| 20 mm | 25 mm | 30 mm | 32 mm | 36 mm |
| 40 mm | 45 mm | 50 mm | 60 mm | |
Stock and supply 400 BHN Rockstar Steel Plate in Thickness 8 to 60mm or Custom With Ultrasonic test as per SA578 LEVEL-B
| Thickness in mm | Width | Length |
|---|---|---|
| 8 | 2000 to 2500 mm | As Per Client Requirement |
| 10 | ||
| 12 | ||
| 14 | ||
| 16 | ||
| 20 | ||
| 25 | ||
| 30 | ||
| 32 | ||
| 36 | ||
| 40 | ||
| 45 | ||
| 50 | ||
| 60 |

Rockstar 400 High Strength Steel Plate
- Method: Hot-Rolled (HR)

Rockstar 400 Liner Plate
- Cutting: Plasma, Laser

Rockstar 400 Wear Resistant Steel Plate
- Treatment: Quenched and Tempered
| Rockstar 400 Chemical Composition (%) | |||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Plate | P | Si | C | Mn | al | Cr | B | S | Nb+Ti+V | N | Mo | Ni | B | CET | CEV |
| thickness mm | max % | max % | max % | max % | min % | max % | max % | max % | max % | max % | max % | max % | max % | typv | typv |
| 8 to 60 mm | 0.025 | 0.70 | 0.30 | 1.60 | 0.02 | 1.80 | 0.0050 | 0.010 | 0.25 | 0.012 | 0.50 | 1.20 | 0.004 | 0.33 | 0.57 |
| Product | Hardness (HBW) | Width (mm) | Thickness (mm) | Length (mm) |
|---|---|---|---|---|
| Plate | 360 to 430 | 2000 to 2500 | 8 to 60 | 6000 to 12000 |
| Plate | 360 to 430 | 2000 to 2500 | 8 to 60 | 6000 to 12000 |
| Sheet | 360 to 430 | 2000 to 2500 | 8 to 60 | 6000 to 12000 |
| Plate | 360 to 430 | 2000 to 2500 | 8 to 60 | 6000 to 12000 |
Buy Rockstar 400 Wear Resistant Steel Plate Stock For Application like Liners for Truck Beds and Mining
- Hoppers
- Liners for Truck Beds
- Crushers
- Buckets
- Excavators and Conveyor Troughs
- Chutes
- Trash Truck Bottoms
- Concrete Mixer Drums
- Dump Trailers
- Street Sweepers
- Bucket Lips
Find Reliable Source Of Rockstar 400 Steel Plate & Wear and abrasion Resistant Steel Plate As Per Stanadrds With Different Heat Treatment and Dimensional Tolerances
| USED FOR | DIMENSIONS | STANDARDS |
|---|---|---|
| Wear and Abrasion Resistant | W: 2000 to 2500 mm T: 8 to 60 mm L: Up to 12000 mm |
EN 10029 Rockstar 400 IS 18809_ISAR_400EN 10163-2 |
| Grade Name | Rockstar 400 |
|---|---|
| Hardness Level | 360 to 430 BHN |
- Submerged Arc Welding
- Manual Electric Welding
- Inert Gas Welding
| Delivery Condition | |
|---|---|
| Quenched / Quenched and Tempered |
|
| Surface Condition |
|
- Weldability
- Formability
- Heat Treatment
- Toughness
- Composition
| Grade & Thickness | Charpy V-Notch Impact Toughness (Min) | Tensile Strength (Min-MPa) | Yield Strength (Min-MPa) | % Elongation (GL = 50 mm) |
|---|---|---|---|---|
| Rockstar 400 Typically Value For 20mm Plate | 27 Joules min Bend Dia.4T | 1150 MPa | 900 MPa | 8% Min. and 5.65 Sqrt. (Area) GL |
| Minimum inner bend rad | |||
|---|---|---|---|
| Bend angle (In degree) | Bend radius is dependent on the direction of bending to rolling direction (t = Plate thickness) | Parallel to rolling direction | Transverse to rolling direction |
| 180 | Rockstar 400 | 4xt | 3xt |
| Length and Width | -0/+20mm |
|---|---|
| Thickness | As per EN 10029 : Class B Table 1 |
| Surface Properties | As per EN 10163-2, Class A Subclass 3 |
| Plate Ultrasonic Testing | SA578 LVB >=10MM & AMNSIL_UT_L_B<=10mm Which is inline With SA578LVB |
| Cutting Process | Preheating | Excess Preheating |
|---|---|---|
| Plasma, and Laser | 100 to 150°C For Plate Thicker Than 40 mm | Above 200°C |
Export to Below Countries